317 stainless steel is a highly corrosion-resistant material, commonly used in environments that require resistance to both oxidation and corrosion, such as chemical processing, food production, and marine environments.
| 3/16″ | 1/4″ | 5/16″ | 3/8″ | 1/2″ | 5/8″ | 3/4″ | 7/8″ | 1″ | 1 1/8″ |
|---|---|---|---|---|---|---|---|---|---|
| 4.8mm | 6.3mm | 7.9mm | 9.5mm | 12.7mm | 15.9mm | 19mm | 22.2mm | 25.4mm | 28.6mm |
| 1 1/4″ | 1 1/2″ | 1 3/4″ | 2″ | 2 1/4″ | 2 1/2″ | 2 3/4″ | 3″ | 3 1/2″ | 4″ |
| 31.8mm | 38.1mm | 44.5mm | 50.8mm | 57.2mm | 63.5mm | 69.9mm | 76.2mm | 88.9mm | 101.6mm |
| Element | Range (wt%) |
|---|---|
| Iron (Fe) | Balance |
| Chromium (Cr) | 18.0 – 20.0 |
| Nickel (Ni) | 11.0 – 15.0 |
| Molybdenum (Mo) | 3.0 – 4.0 |
| Manganese (Mn) | 0.0 – 2.0 |
| Silicon (Si) | 0.0 – 1.0 |
| Carbon (C) | ≤ 0.08 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Property | Value |
|---|---|
| Density | ~7.98 g/cm³ (7980 kg/m³) |
| Melting Point | ~1400 – 1450°C (2552 – 2642°F) |
| Thermal Conductivity | ~15.1 W/m·K |
| Specific Heat Capacity | ~500 J/kg·K |
| Young’s Modulus | ~200 GPa (29,000 ksi) |
| Poisson’s Ratio | ~0.27 – 0.30 |
| Electrical Resistivity | ~0.72 x 10⁻⁸ Ω·m |
| Coefficient of Thermal Expansion | ~16.5 x 10⁻⁶ /°C (9.2 x 10⁻⁶ /°F) |
| Ultimate Tensile Strength | ~550 MPa (80 ksi) |
| Property | Value |
|---|---|
| Ultimate Tensile Strength | ~550 MPa (80 ksi) |
| Yield Strength | ~290 MPa (42 ksi) |
| Elongation | ~40% |
| Reduction of Area | ~60% |
| Hardness (Rockwell B) | ~85 – 95 HRB |
| Modulus of Elasticity (Young’s Modulus) | ~200 GPa (29,000 ksi) |
| Shear Strength | ~280 MPa (41 ksi) |
| Poisson’s Ratio | ~0.27 – 0.30 |
| Fatigue Strength | ~275 MPa (40 ksi) |
| Impact Toughness | Excellent at room temperature and down to cryogenic temperatures |